6 solutions to the orange peel pattern of ceramic water cup products

1. When glazing, don’t be in a hurry, too fast will be uneven and easy to produce air bubbles;

2. When applying the glaze of painted ceramics, the sprayed glaze becomes granular, and it is enough to feel like it is snowing;

3. When applying the biscuit glaze, apply a thickness of 0.4-0.8mm;

4. Before entering the kiln, check whether the green body is completely dry. If it is not dry, it must be made up when firing the kiln. The water discharge period is set at 0-300 degrees, and it is enough to burn for about 2 hours;

5. The oxidative decomposition period is 300-1000°C. During the oxidation period, the average temperature needs to be raised in 1 minute to be 2-3°C. If the temperature rises quickly, the oxidation will be insufficient;

6. When firing, set the firing temperature according to the melting point of the glaze;

The glazing process seems to be simple, but it is really not true in practice. There is no objective reference to make gestures. The depth of skill depends on experience and eyesight. Practice your kung fu well, and then exert your strength!

 